Blue Origin Contracts Aerolloy Technologies for BE-4 Engine Superalloy Castings
SPACE ECONOMY
Blue Origin has contracted Aerolloy Technologies Limited to develop Nickel-based superalloy castings for its BE-4 engines, which power the New Glenn heavy-lift launch vehicle. The agreement, announced on January 8, 2026, focuses on producing high-integrity castings for the engine's Liquid Oxygen systems and aligns with India's initiatives to enhance its role in the global space propulsion market.

Jan 11, 2026, 9:39 AM